Template:Announcements: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
IBD up
Line 1:
<startfeed />
 
=====Stepper #3 (ASML: intermittentDUV) - alignmentDown, failures=====update
=====
I have determined that the laser used for Alignment is failing, the power is low and it flickers.
Sorry to say, I was not able to remedy the wafer handling pick up issue, and the system still intermittent,y fails to pick up a wafer correctly. I might have a temporary workaround by using specific slots and such, but I would need to help you do this.
I have ordered a replacement for the possibly failing WH board causing this.
 
Let me know if you want to try and run one or two wafers through and I might be able to help you do this, but I was having difficulty getting exposures to run properly.
We will order a replacement ASAP and schedule an ASML engineering visit to install + calibrate a new one.
 
To fix the main alignment, laser issue, Asml engineers will be on site Monday and Tuesday next week, so the tool will be down during that time to perform the repairs.
In the mean time, I'm sorry to say that you will see intermittent "reject" wafers. Please see email for info on recovering from this error.
 
// [[User:John_dMehalana v|Demis D.Vraj JohnMehalana]] 1817:1446, 611 September 2024 (PDT)
 
=====LAB OPEN=====

Revision as of 00:46, 12 September 2024

=====Stepper #3 (ASML DUV) - Down, update

=

Sorry to say, I was not able to remedy the wafer handling pick up issue, and the system still intermittent,y fails to pick up a wafer correctly. I might have a temporary workaround by using specific slots and such, but I would need to help you do this. I have ordered a replacement for the possibly failing WH board causing this.

Let me know if you want to try and run one or two wafers through and I might be able to help you do this, but I was having difficulty getting exposures to run properly.

To fix the main alignment, laser issue, Asml engineers will be on site Monday and Tuesday next week, so the tool will be down during that time to perform the repairs.

//Vraj Mehalana 17:46, 11 September 2024 (PDT)

LAB OPEN

House vacuum repair has been completed, lab is open for use. //Demis D. John 12:13, 6 September 2024 (PDT)

MLA150: Down

Heidelberg engineer is on site working on repair, we will update as we learn more. // Demis D. John 12:13, 6 September 2024 (PDT)

IBD is UP

The IBD is back up.

With Mike Silva's help, the fixture was recovered without having to vent the loadlock/chamber. // Demis D. John 20:48, 6 September 2024 (PDT)

Suss SB6-8E

When the vendor came in to install the new top heater he wasn't able to get the z-axis (elevator motor) to move. He was able to install the new heater and do a PM on the rest of the tool. We are ordering a new z-axis controller on the recommendation of the vendor. If all goes well this should solve the issue and make the bonder fully operational. I'll send out an email once the new controller has been installed.

-Aidan //Vraj Mehalana 12:43, 3 September 2024 (PDT)


EBeam#2: Down

Good news is we have repaired and reinstalled the hoist, thanks Mike B. and Bill. I have tested it and everything looks good.

However, the repaired bell jar mount is not sliding down the hoist pole like it should. Since the repair involved some welding to the collar that slides down the hoist pole, we surmise that the concentricity was affected by the heat. The mount is back at the machine shop getting honed out. I should have it back to test late today/early tomorrow but it may have to go back again. Once it is able to slide on properly the tool should be up shortly thereafter.

-Lee // Demis D. John 14:24, 27 August 2024 (PDT)

YES EcoClean: 3kW only

I swapped out the RF generator and the tool is working again. I am getting repeated CCP warnings for the 0.7kW recipes so we will need to look into that further.

System is up for 3kW recipes only.

DO NOT run 0.7kW recipes until further notice!!

-- Lee Sawyer//Demis D. John 11:31, 23 August 2024 (PDT)

ICP1 Down

The board we were waiting on arrived, but it did not resolve the tool issue. We are working with Panasonic on the next steps. //Vraj Mehalana 14:17, 1 March 2024 (PST)

Lab Access Changes: Symmetry App

The iris scanner has been decommissioned. Please use the card reader which supports:

-Physical card

-Mobile phone via Symmetry App

//Vraj Mehalana 16:59, 14 June 2024 (PDT)