*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]] | *[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]] | ||
− | =[[XeF<sub>2</sub> Etch (Xetch | + | =[[XeF<sub>2</sub> Etch (Xetch)]]= |
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]] | *[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]] |