Line 8: Line 8:


=[[CAIBE (Oxford Ion Mill)]]=
=[[CAIBE (Oxford Ion Mill)]]=
*[[media:*[[media:|Pt Etch Recipe]]|Pt Etch Recipe]]
*[[media:*[[media:42-Etching_Platinum_using_Oxford_Ion_Mill_Tool.pdf|Pt Etch Recipe]]|Pt Etch Recipe]]