Unaxis Test Recipe Page: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
test |
(No difference)
|
Latest revision as of 22:19, 20 April 2018
| 0.264 | 2.57 | 2.59 | 2.61 | 82.90223 |
| 0.256 | 2.54 | 2.33 | 2.35 | 82.51937 |
| 0.3 | 2.64 | 2.62 | 2.66 | 80.05097 |
| 0.296 | 2.61 | 2.34 | 2.36 | 82.53525 |
| 0.296 | 2.63 | 2.9 | 2.92 | 83.29001 |