Test Data of etching SiO2 with CHF3/CF4: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
add a data table |
add a data table |
||
| Line 1: | Line 1: | ||
{| class="wikitable" |
{| class="wikitable" |
||
| colspan="5" |ICP#2: 0.5Pa, 50/ |
| colspan="5" |ICP#2: 0.5Pa, 50/900W, CHF3/CF4=10/30 sccm, time=210 sec |
||
|- |
|- |
||
|Date |
|Date |
||
Revision as of 15:13, 9 October 2018
| ICP#2: 0.5Pa, 50/900W, CHF3/CF4=10/30 sccm, time=210 sec | ||||
| Date | Sample# | Etch Rate (nm/min) | Etch Selectivity (SiO2/PR) | Averaged Sidewall Angle (o) |
| 10/5/2018 | SiO2#02 | 160 | 1.2 | 82.1 |