Test Data of etching SiO2 with CHF3/CF4: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
No edit summary |
No edit summary |
||
| Line 20: | Line 20: | ||
| |
| |
||
|} |
|} |
||
[https://www.nanotech.ucsb.edu/wiki/images/f/f9/SiO2_Etch_using_ICP2-no_O2-a.pdf] |
|||
Revision as of 18:43, 29 January 2019
| ICP#2: 0.5Pa, 50/900W, CHF3/CF4=10/30 sccm, time=210 sec | ||||
| Date | Sample# | Etch Rate (nm/min) | Etch Selectivity (SiO2/PR) | Averaged Sidewall Angle (o) |
| 10/5/2018 | SiO2#02 | 160 | 1.2 | 82.1 |
| 1/28/19 | I21901 | 146 | 1.23 | |