add a pic |
save a data |
||
| Line 24: | Line 24: | ||
|[https://www.nanotech.ucsb.edu/wiki/images/f/f9/SiO2_Etch_using_ICP2-no_O2-a.pdf] |
|[https://www.nanotech.ucsb.edu/wiki/images/f/f9/SiO2_Etch_using_ICP2-no_O2-a.pdf] |
||
|- |
|- |
||
|3/6/ |
|3/6/2019 |
||
|I21904 |
|I21904 |
||
|151 |
|151 |
||
|1.23 |
|1.23 |
||
|85.6 |
|85.6 |
||
| |
|||
|[[:File:SiO2 Etch using ICP2 no O2-3-06-2019.pdf]] |
|||
|} |
|} |
||