This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter. |
This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter. |
||
Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc. |
Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc. |
||
=Detailed Specifications= |
==Detailed Specifications== |
||
*DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 watts and can operate in either constant intensity or constant power mode |
*DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 watts and can operate in either constant intensity or constant power mode |
||
*The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample |
*The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample |
||
| Line 22: | Line 23: | ||
*Lamps are nominally rated for 400 hours |
*Lamps are nominally rated for 400 hours |
||
*A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation |
*A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation |
||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
| ⚫ | |||
[[image:DUV-System-Spectra.png|thumb|none|600px|DUV Exposure System Spectra]] |
[[image:DUV-System-Spectra.png|thumb|none|600px|DUV Exposure System Spectra]] |
||
== Documentation == |
|||
* [https://signupmonkey.ece.ucsb.edu/wiki/images/2/27/DUV_Flood_Expose_SOP.pdf DUV Flood Expose Standard Operating Procedure] |
|||
Revision as of 22:26, 11 September 2019
<nowiki>Insert non-formatted text here<nowiki>Insert non-formatted text here</nowiki></nowiki>
|
About
This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter.
Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc.
Detailed Specifications
- DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 watts and can operate in either constant intensity or constant power mode
- The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample
- Exposure can be performed on a 4" wafer
- Lamps are nominally rated for 400 hours
- A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation