Line 1: Line 1:
Pressure drop indicates completion of etch. Once pressure flattens etching is complete.
Pressure drop indicates completion of etch. Once pressure flattens etching is complete.

[[File:YES-SPR220vsTemp.jpg|578x578px]][[File:PPR220-7 Etch Rates (nm min) vs. Temp(C) Recipe STD O2only 3KW-3min-Temp (1).png|thumb|571.804x571.804px|alt=|left]]
[[File:YES-SPR220vsTemp.jpg|578x578px]]

<br />
<br />

Revision as of 16:32, 5 June 2023

Pressure drop indicates completion of etch. Once pressure flattens etching is complete.