Pressure drop indicates completion of etch. Once pressure flattens etching is complete. |
Pressure drop indicates completion of etch. Once pressure flattens etching is complete. |
||
[[File:YES-SPR220vsTemp.jpg|578x578px]] |
[[File:YES-SPR220vsTemp.jpg|578x578px]]<br /> |
||
<br /> |
|||
[[File:PPR220-7 Etch Rates vs Temperature.jpg|left|thumb|572.812x572.812px|Positive PR 220-7 etch rates vs set point temperature]] |
|||