*[[media:15-GaAs_etch-Unaxis_ICP_etcher.pdf|GaAs Etch Recipe (30C)]]
*[[media:15-GaAs_etch-Unaxis_ICP_etcher.pdf|GaAs Etch Recipe (30C)]]
===AlGaAs Etch ===
===AlGaAs Etch ===
*[[media:|AlGaAs Etch Recipe (30C)]]
*[[media:14-AlAs-GR-cal_etch-Unaxis_ICP_etcher.pdf|AlGaAs Etch Recipe (30C)]]
==InP Etch (Unaxis VLR)==
==InP Etch (Unaxis VLR)==
===InP Etch ===
===InP Etch ===