= About =
= About =


This ICP is a time machine. It can literally take you into the future of nanotechnology. Just look at it. Amazing!
⚫
This is a three-chamber tool for etching of a variety of materials. Chamber one is configured as an ICP etching tool with 1000 W ICP power, 500 W RF substrate power, and RT - 80°C operation with back-side He cooling and an electrostatic chuck to maintain controlled surface temperatures during etching. This chamber has Cl<sub>2</sub>, BCl<sub>3</sub>, CF<sub>4</sub>, CHF<sub>3</sub>, SF<sub>6</sub>, Ar, N<sub>2</sub>, and O<sub>2 </sub>for gas sources and can be used to etch a variety of materials from SiO<sub>2</sub> to metals to compound semiconductors. The chamber evacuated with a 2000 lpm Osaka Vacuum magnetically levitated turbo pump, allowing for fast pump down. Chamber two is a 2000 W ICP chamber configures for plasma etching of photoresist and other materials such as BCB. The substrate is not biased and the chamber has CF<sub>4</sub> and O<sub>2</sub> for the gases. Chamber three is a DI rinsing chamber for rinsing off any etch byproducts before removing the sample from the system. The system accepts 6” wafers or pieces mounted to the wafers. In Automatic mode, multiple wafers can be run through automatically with the cassette-based system.of low-stress Nitride films.

⚫
This is a single-chamber tool for etching of a variety of materials. The chamber is configured as an ICP etching tool with 1250 W ICP power, 600 W RF substrate power, and RT-80°C operation with back-side He cooling and an electrostatic chuck to maintain controlled surface temperatures during etching. This chamber has Cl<sub>2</sub>, BCl<sub>3</sub>, CF<sub>4</sub>, CHF<sub>3</sub>, SF<sub>6</sub>, Ar, N<sub>2</sub>, He, and O<sub>2</sub> for gas sources and can be used to etch a variety of materials from SiO<sub>2</sub> to metals to compound semiconductors. The chamber evacuated with a 2000 lpm Osaka Vacuum magnetically levitated turbo pump, allowing for fast pump down. The system accepts 6” wafers (JEIDA Std) or pieces mounted to the wafers.


= Detailed Specifications =
= Detailed Specifications =


*1000 W ICP source, 500 W RF Sample Bias Source in etching chamber
*1250 W ICP source, 600 W RF Sample Bias Source in etching chamber
*RT - 80°C sample temperature for etching
*RT - 80°C sample temperature for etching
⚫
*Etch pressure from 0.1 Pa to 5 Pa (0.75 mT - 37.5 mT)
*Optimal Emission Monitoring
⚫
*Cl<sub>2</sub>, BCl<sub>3</sub>, CF<sub>4</sub>, CHF<sub>3</sub>, SF<sub>6</sub>, Ar, N<sub>2</sub>, He, and O<sub>2</sub> in etch chamber
⚫
*Etch pressure from 0.1 Pa to 5 Pa (0.75 mT - 37.5 mT)
⚫
*Cl<sub>2</sub>, BCl<sub>3</sub>, CF<sub>4</sub>, CHF<sub>3</sub>, SF<sub>6</sub>, Ar, N<sub>2</sub>, and O<sub>2</sub> in etch chamber
*2000 W ICP ashing chamber
*RT - 250°C sample temperature for ashing
*Ashing pressures 50 mT - 500 mT
*O<sub>2</sub>, N<sub>2</sub>, CF<sub>4</sub>, H<sub>2</sub>O Vapor for ashing chamber
*Multiple 6” diameter wafer capable system
*Pieces possible by mounting to 6” wafer
*Pieces possible by mounting to 6” wafer
*Load-Locked

*Up to 20 steps per recipe

*Laser monitor with 679.60nm wavelength


=Documentation=
=Documentation=

Revision as of 14:32, 14 June 2015

ICP Etch 1 (Panasonic E646V)
Tool Type Dry Etch
Location Bay 2
Supervisor Don Freeborn
Supervisor Phone (805) 893-7975
Supervisor E-Mail dfreeborn@ece.ucsb.edu
Description ?
Manufacturer Panasonic Factory Solutions, Japan
Dry Etch Recipes
Sign up for this tool


About

This ICP is a time machine. It can literally take you into the future of nanotechnology. Just look at it. Amazing!

This is a single-chamber tool for etching of a variety of materials. The chamber is configured as an ICP etching tool with 1250 W ICP power, 600 W RF substrate power, and RT-80°C operation with back-side He cooling and an electrostatic chuck to maintain controlled surface temperatures during etching. This chamber has Cl2, BCl3, CF4, CHF3, SF6, Ar, N2, He, and O2 for gas sources and can be used to etch a variety of materials from SiO2 to metals to compound semiconductors. The chamber evacuated with a 2000 lpm Osaka Vacuum magnetically levitated turbo pump, allowing for fast pump down. The system accepts 6” wafers (JEIDA Std) or pieces mounted to the wafers.

Detailed Specifications

  • 1250 W ICP source, 600 W RF Sample Bias Source in etching chamber
  • RT - 80°C sample temperature for etching
  • Etch pressure from 0.1 Pa to 5 Pa (0.75 mT - 37.5 mT)
  • Cl2, BCl3, CF4, CHF3, SF6, Ar, N2, He, and O2 in etch chamber
  • Pieces possible by mounting to 6” wafer
  • Load-Locked
  • Up to 20 steps per recipe
  • Laser monitor with 679.60nm wavelength

Documentation