{| class="wikitable" |
|||
| colspan="5" |ICP#2: 0.5Pa, 50/900W, CHF3/CF4=10/30 sccm, time=210 sec |
|||
|- |
|||
|Date |
|||
|Sample# |
|||
|Etch Rate (nm/min) |
|||
|Etch Selectivity (SiO2/PR) |
|||
|Averaged Sidewall Angle (<sup>o</sup>) |
|||
|- |
|||
|10-8-2018 |
|||
|SiO2#02 |
|||
|160 |
|||
|1.23 |
|||
|82.1 |
|||
|- |
|||
|1/28/2019 |
|||
|I21901 |
|||
|146 |
|||
|1.23 |
|||
| |
|||
|} |
|||
[https://www.nanotech.ucsb.edu/wiki/index.php/File:SiO2_Etch_using_ICP2-no_O2-a.pdf File:SiO2 Etch using ICP2-no O2-a.pdf] |
|||