Other Dry Etching Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Ningcao (talk | contribs)
Ningcao (talk | contribs)
→CAIBE (Oxford Ion Mill): add a recipe file
Line 12: Line 12:
*[https://wiki.nanotech.ucsb.edu/w/images/e/e3/44-Etching_Gold_with_Al2O3_Mask_using_Oxford_Ion_Mill_Tool.pdf Au Etch Recipe]
*[https://wiki.nanotech.ucsb.edu/w/images/e/e3/44-Etching_Gold_with_Al2O3_Mask_using_Oxford_Ion_Mill_Tool.pdf Au Etch Recipe]
*[https://wiki.nanotech.ucsb.edu/w/images/f/f1/45-Etching_Nickel_with_Al2O3_Mask_using_Oxford_Ion_Mill_Tool.pdf Ni Etch Recipe]
*[https://wiki.nanotech.ucsb.edu/w/images/f/f1/45-Etching_Nickel_with_Al2O3_Mask_using_Oxford_Ion_Mill_Tool.pdf Ni Etch Recipe]
*[https://wiki.nanotech.ucsb.edu/wiki/File:InP_Etching_result-CAIBE.docx InP Etch Recipe]
*InP Etch Recipe


=Misc=
=Misc=

Revision as of 22:14, 31 July 2020