Line 9: Line 9:
|SEM Image
|SEM Image
|-
|-
|11/5/2021
|
|SOFL01
|
|
|136
|
|1.2
|
|
|
|

Latest revision as of 20:43, 9 November 2021

Flourine ICP: 3.8mT, 50/900W, CF4/CHF3=30/10sccm, time=210 sec
Date Sample# Etch Rate (nm/min) Etch Selectivity (SiO2/PR) Averaged Sidewall Angle (o) SEM Image
11/5/2021 SOFL01 136 1.2