ICP-PECVD (Unaxis VLR): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Zwarburg (talk | contribs)
Created page with "{{tool|{{PAGENAME}} |picture=UnaxisVLR.jpg |type = Vacuum Deposition |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay 1 |email=bosch@ece.ucsb.edu |description = High Den…"
 
Zwarburg (talk | contribs)
No edit summary
Line 20: Line 20:
*Multiple 4” diameter wafer capable system
*Multiple 4” diameter wafer capable system
*Pieces possible by mounting or placing on 4 ” wafer
*Pieces possible by mounting or placing on 4 ” wafer

=Documentation=
*[[media:UnaxisVLRInstructions.pdf|Operating Instructions]]

Revision as of 14:52, 28 June 2012

ICP-PECVD (Unaxis VLR)
File:UnaxisVLR.jpg
Tool Type Vacuum Deposition
Location Bay 1
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description High Density ICP PECVD
Manufacturer Unaxis
Vacuum Deposition Recipes


About

This system is configured as an ICP PECVD deposition tool with 1000 W ICP power, 600 W RF substrate power, and RT-350°C operation. This chamber has 100% SiH4, N2, O2, and Ar for gas sources. The high density PECVD produces a more dense, higher quality SiO2 and Si3N4, as compared with conventional PECVD. With the high density plasma, deposition of high quality films can be done down to below 50°C for processes requiring lower temperatures. Stress compensation for silicon nitride is characterized.

Detailed Specifications

  • 1000W ICP source, 600W RF Sample Bias Source in etching chamber
  • RT - 350°C sample temperature
  • 100% SiH4, Ar, N2, O2
  • Multiple 4” diameter wafer capable system
  • Pieces possible by mounting or placing on 4 ” wafer

Documentation