Oxford ICP Etcher (PlasmaPro 100 Cobra): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
No edit summary
Line 50: Line 50:
*{{file|Oxford PLasmaPro Operating Instructions.pdf|Oxford PlasmaPro Operating Instructions}}
*{{file|Oxford PLasmaPro Operating Instructions.pdf|Oxford PlasmaPro Operating Instructions}}
*[[Laser Etch Monitoring|Laser Etch Monitoring procedures]]
*[[Laser Etch Monitoring|Laser Etch Monitoring procedures]]
*Online Training Video:

**["G:\Shared drives\NanoFab Equipment Group\Nanofab Equip Standard Operating Procedures\3.0 Dry Etch\3.18 Oxford PlasmaPro 100 Cobra 300\Training Video\Oxford Plasma Pro 100 Cobra 300 Training Video 2.mp4" <u>Oxford Cobra 300 Training</u>]
**'''Important:''' ''This video is for reference only, and does not give you authorization to use the tool. You must be officially authorized by the supervisor before using this machine.''


==Recipes==
==Recipes==

Revision as of 16:16, 4 January 2022

Oxford ICP Etcher (PlasmaPro 100 Cobra)
Tool Type Dry Etch
Location Bay 2
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description ICP Etches for III-V/ALE
Manufacturer Oxford Instruments
Model PlasmaPro 100 Cobra 300
Materials InP, GaAs, GaN, Silicon ALE
Dry Etch Recipes


About

The Oxford PlasmaPro 100 Cobra 300 is intended for etching InP-based, GaAs-baased and GaN-based epitaxies, in addition to Atomic Layer Etching (ALE) processes. The system has a load lock, wide temperature range with rapid heating/cooling, Inductively Coupled Plasma (ICP) coil and a capactively coupled substrate HF (13.56MHz) The fixturing is configured for 4" diameter Si wafers and uses a clamp to hold the sample on the RF chuck. Small pieces may be placed on Silicon carrier wafers, with or without mounting adhesive. Helium back-side cooling is used to keep the sample cool during the etch, but pieces do heat up when placed on carriers.

The in-situ laser monitor installed on this system allows for repeatable etches and endpoint detection via continuous optical monitoring of the wafer reflectivity in a user-determined location, through a porthole on the chamber. The system also has an in situ optical emission monitor for plasma spectroscopy, utilized for chamber clean endpoint detection.

Detailed Specifications

  • Temperature Range: –150°C to +400°C
  • Gases Available: CH4, H2, Ar, Cl2, BCl3, SF6, SiCl4, O2, N2
  • ICP Power (max): 3000 W
  • RF Power (max): 600 W
  • He-back-side cooling
  • 100mm wafer held down with ceramic clamp., single-load
    • Users may place pieces onto carrier wafer with or without adhesive. Standard recipes use no adhesive.
    • Pieces must be >7mm from edge of carrier to avoid wafer-clamping mechanism.
  • Windows-based Cortex software control of process and wafer handling
  • Allowed Materials:
    • InP-based epitaxies - qualified and ready
    • GaAs-baased epitaxies - discuss with staff
    • GaN-based epitaxies - discuss with staff
    • GaSb-based epitaxies - discuss with staff
    • Atomic Layer Etching on select materials - discuss with staff
  • Standard masking materials include:
    • SiO2
    • Si3N4
    • photoresist (at << 100°C).

Other materials can be exposed to the chamber only with staff approval.

  • Laser monitoring with camera and etch simulation software: Intellemetrics LEP 500
  • Optical Emission Spectroscopy (Ocean Optics) for endpoint detection of chamber cleans & etches - integrated into Oxford software

Documentation

  • Oxford PlasmaPro Operating Instructions
  • Laser Etch Monitoring procedures
  • Online Training Video:
    • ["G:\Shared drives\NanoFab Equipment Group\Nanofab Equip Standard Operating Procedures\3.0 Dry Etch\3.18 Oxford PlasmaPro 100 Cobra 300\Training Video\Oxford Plasma Pro 100 Cobra 300 Training Video 2.mp4" Oxford Cobra 300 Training]
    • Important: This video is for reference only, and does not give you authorization to use the tool. You must be officially authorized by the supervisor before using this machine.

Recipes