Line 2: Line 2:


[[File:YES-SPR220vsTemp.jpg|578x578px]]
[[File:YES-SPR220vsTemp.jpg|578x578px]]

<br />
[[File:PPR220-7 Etch Rates vs Temperature.jpg|left|thumb|572.812x572.812px|Positive PR 220-7 etch rates vs set point temperature]]



<br />
<br />

Revision as of 16:35, 5 June 2023

Pressure drop indicates completion of etch. Once pressure flattens etching is complete.


Positive PR 220-7 etch rates vs set point temperature