DUV Flood Expose: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
Created page with "{{tool|{{PAGENAME}} |picture=DUV.jpg |type = Lithography |super= Mike Silva |phone=(805)839-3918x219 |location=Bay 6 |email=silva@ece.ucsb.edu |description = Deep UV Flood Expose…" |
No edit summary |
||
| Line 22: | Line 22: | ||
*Lamps are nominally rated for 400 hours |
*Lamps are nominally rated for 400 hours |
||
*A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation |
*A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation |
||
=Spectra Images= |
|||
==Aligner with No Filter== |
|||
[[image:DUV-Spectra-No-Filter.png|thumb|none|600px|Aligner with No Filter]] |
|||
==Aligner with Filter for i-line Exposure== |
|||
[[image:DUV-Spectra-With-Filter.png|thumb|none|600px|Aligner with Filter for i-line Exposure]] |
|||
==DUV Exposure System Spectra== |
|||
[[image:DUV-System-Spectra.png|thumb|none|600px|DUV Exposure System Spectra]] |
|||
Revision as of 04:24, 28 June 2012
|
About
This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter.
Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc.
Detailed Specifications
- DUV wavelengths are 200-260 nm; the lamp power is limited to either 1250 or 2100 watts and can operate in either constant intensity or constant power mode
- The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample
- Exposure can be performed on a 4" wafer
- Lamps are nominally rated for 400 hours
- A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation
Spectra Images
Aligner with No Filter

Aligner with Filter for i-line Exposure

DUV Exposure System Spectra