{{recipes|Dry Etching}}
⚫
=[[XeF2 Etch (Xetch)]]=
⚫
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]]





{{recipes|Dry Etching}}
{{recipes|Dry Etching}}
=[[ICP Etch 1 (Panasonic E626I)]]=
=[[ICP Etch 1 (Panasonic E626I)]]=
Line 21: Line 29:
===InP Etch (H<sub>2</sub> Ar)===
===InP Etch (H<sub>2</sub> Ar)===
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]

⚫
=[[XeF2 Etch (Xetch)]]=
⚫
*[[media:06-XeF2-etch-recipe.pdf|Si Etch Recipe]]