ICP Etching Recipes: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Ningcao (talk | contribs)
Ningcao (talk | contribs)
Line 21: Line 21:
===InP Etch (H<sub>2</sub> Ar)===
===InP Etch (H<sub>2</sub> Ar)===
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
*[[media:UNAXIS-VLR-InP-Etch-Ar-200C-Recipe.pdf|InP Etch Recipe (H<sub>2</sub> Ar 200C)]]
==GaN Etch (Unaxis VLR)==
*[[media:|GaN Etch Recipe (85C)]]

Revision as of 21:12, 24 September 2013