=Example Wet Etching Table (Include All Materials)=
How to use the wet etch table:
How to use the wet etch table:


Line 5: Line 8:


This multiple entry method may seem laborious for the person entering a new etch, however the power of sorting by selective materials and chemicals in a table with all materials is great.
This multiple entry method may seem laborious for the person entering a new etch, however the power of sorting by selective materials and chemicals in a table with all materials is great.

⚫
=Example Wet Etching Table (Include All Materials)=


{| class="wikitable sortable"
{| class="wikitable sortable"

Revision as of 18:27, 6 November 2013


Example Wet Etching Table (Include All Materials)

How to use the wet etch table:

When entering a new etch into the table make a row for every etchant used in the solution such that the information can be sorted by etchant. For example, the InP etch HCl:H3PO4(1:3) and H3PO4:HCl(3:1). Likewise, if etch is known to be selective to multiple materials the etch should have a row for each material. For example HCl:H3PO4(1:3) is selective to both InGaAs and InGaAsP.

This multiple entry method may seem laborious for the person entering a new etch, however the power of sorting by selective materials and chemicals in a table with all materials is great.

Material Etchant Rate (nm/min) Anisotropy Selective to Selectivity Ref. Notes Confirmed by Extra column
InP HCl:H3PO4(1:3) ~1000 Highly InGaAs High [Lamponi (p.102)] Example Jon Doe Example
InP HCl:H3PO4(1:3) ~1000 Highly InGaAsP High [Lamponi (p.102)] Example Jon Doe Example
InP H3PO4:HCl(3:1) ~1000 Highly InGaAs High [Lamponi (p.102)] Example Jon Doe Example
InP H3PO4:HCl(3:1) ~1000 Highly InGaAsP High [Lamponi (p.102)] Example Jon Doe Example

Compound Semiconductor Etching

Metal Etching

Silicon etching

Dielectric etching

Organic removal

Gold Plating

Chemi-Mechanical Polishing (CMP)