1
PECVD 1 (PlasmaTherm 790)
1.1
SiN deposition (PECVD #1)
1.2
SiO
2
deposition (PECVD #1)
2
PECVD 2 (Advanced Vacuum)
2.1
SiN deposition (PECVD #2)
2.2
SiO
2
deposition (PECVD #2)
3
ICP-PECVD (Unaxis VLR)
PECVD 1 (PlasmaTherm 790)
SiN deposition (PECVD #1)
SiN Deposition Recipe
SiN Deposition Particle Thickness Data
SiO
2
deposition (PECVD #1)
SiO
2
Deposition Recipe
SiO
2
Deposition Particle Thickness Data
PECVD 2 (Advanced Vacuum)
SiN deposition (PECVD #2)
SiN Deposition Recipe
SiN Deposition Particle Thickness Data
SiO
2
deposition (PECVD #2)
SiO
2
Deposition Recipe
SiO
2
Deposition Particle Thickness Data
ICP-PECVD (Unaxis VLR)
Category
:
Recipes
Navigation menu
Personal tools
Create account
Log in
Namespaces
Page
Discussion
English
Views
Read
View source
View history
More
Search
InvisibleMenu
QuickLinks
Lab Rules
Common Questions/FAQ
Staff List
Equipment Signup
Chemicals + MSDS
Protofab
Equipment
Full Tool List
Lithography
Vacuum Deposition
Dry Etch
Wet Processing
Thermal Processing
Packaging
Metrology & Test
Recipes and Data
Lithography
Vacuum Deposition
Dry Etching
Wet Etching
Thermal Processing
Packaging Tools
Data + Info
Process Control Data
Tutorials
Calculators/Utilities
NanoFab Info
Research + Pubs
Tech Talks
Tools
What links here
Related changes
Special pages
Printable version
Permanent link
Page information