ICP Etching Recipes
Jump to navigation
Jump to search
Back to Dry Etching Recipes.
ICP Etch 1 (Panasonic E626I)
SiO2 Etching (Panasonic 1)
Cr Etch (Panasonic 1)
GaN Etch (Panasonic 1)
ICP Etch 2 (Panasonic E640)
SiO2 Etching (Panasonic 2)
ICP-Etch (Unaxis VLR)
InP Etch (Unaxis VLR)
InP Etch
InP Etch (H2 Ar)
GaN Etch (Unaxis VLR)
- [[media:|GaN Etch Recipe (85C)]]