Si Deep RIE (PlasmaTherm/Bosch Etch)
Single-step Si Etching (not Bosch Process!) (Si Deep RIE)
ICP Etch 1 (Panasonic E626I)
SiO2 Etching (Panasonic 1)
Al Etch (Panasonic 1)
Cr Etch (Panasonic 1)
Ti Etch (Panasonic 1)
AlGaAs Etch (Panasonic 1)
GaN Etch (Panasonic 1)
ICP Etch 2 (Panasonic E640)
SiO2 Etching (Panasonic 2)
Al Etch (Panasonic 2)
ICP-Etch (Unaxis VLR)
GaAs Etch
- [[media:|GaAs Etch Recipe (30C)]]