SiO2 Etching Test using CF4/CHF3
| Flourine ICP: 3.8mT, 50/900W, CF4/CHF3=30/10sccm, time=210 sec | |||||
| Date | Sample# | Etch Rate (nm/min) | Etch Selectivity (SiO2/PR) | Averaged Sidewall Angle (o) | SEM Image |
| Flourine ICP: 3.8mT, 50/900W, CF4/CHF3=30/10sccm, time=210 sec | |||||
| Date | Sample# | Etch Rate (nm/min) | Etch Selectivity (SiO2/PR) | Averaged Sidewall Angle (o) | SEM Image |