Gold surface oxidation (darkening) due to O2/N2 plasma; the need for O2 only recipe.

From UCSB Nanofab Wiki
Revision as of 23:14, 9 June 2023 by Ffoong (talk | contribs) (Gold surface darkened after O2/N2 ashing recipe treatment, XPS data showed that Au can oxidize in the high oxidization condition)