File:SEM Image of wafer after PR strip.png
Size of this preview: 800 × 321 pixels. Other resolution: 1,500 × 601 pixels.
Original file (1,500 × 601 pixels, file size: 718 KB, MIME type: image/png)
PR used as mask for 5min Si etch. Followed by PR strip with 2min over etch