File:SEM Image.png
Size of this preview: 800 × 322 pixels. Other resolution: 1,500 × 603 pixels.
Original file (1,500 × 603 pixels, file size: 706 KB, MIME type: image/png)
Wafer had UV6 or UVN30 as mask. 5min Si etch followed by PostBARC Etch/PR Strip (STD)_V2 with 2min over etch
File history
Click on a date/time to view the file as it appeared at that time.
| Date/Time | Thumbnail | Dimensions | User | Comment | |
|---|---|---|---|---|---|
| current | 18:47, 28 January 2025 | 1,500 × 603 (706 KB) | Gopimeena (talk | contribs) |