Si Deep RIE (PlasmaTherm/Bosch Etch)
Single-step Si Etching (not Bosch Process!) (Si Deep RIE)
ICP Etch 1 (Panasonic E626I)
SiO2 Etching (Panasonic 1)
Al Etch (Panasonic 1)
Cr Etch (Panasonic 1)
Ti Etch (Panasonic 1)
AlGaAs Etch (Panasonic 1)
GaN Etch (Panasonic 1)
ICP Etch 2 (Panasonic E640)
SiO2 Etching (Panasonic 2)
Al Etch (Panasonic 2)
GaAs Etch (Panasonic 2)
ICP-Etch (Unaxis VLR)
GaAs Etch
AlGaAs Etch
InP Etch (Unaxis VLR)
InP Etch
InP Etch (H2 Ar)
- InP Etch Recipe (H2 Ar 200C)
- [[media:|InP-InGaAs Etch Profile (H2 Ar 200C)]]