ICP Etching Recipes
Revision as of 15:49, 18 September 2013 by Ningcao (talk | contribs) (→Si-Etch (XeF2 Etch (Xetch)))
Back to Dry Etching Recipes.
ICP Etch 1 (Panasonic E626I)
SiO2 Etching (Panasonic 1)
Cr Etch (Panasonic 1)
GaN Etch (Panasonic 1)
ICP Etch 2 (Panasonic E640)
SiO2 Etching (Panasonic 2)
ICP-Etch (Unaxis VLR)
InP Etch (Unaxis VLR)
InP Etch
InP Etch (H2 Ar)