ICP#1: 0.5Pa, 50/900W, CHF3/CF4=10/30 sccm, time=210 sec | ||||
Date | Sample# | Etch Rate (nm/min) | Etch Selectivity (SiO2/PR) | Averaged Sidewall Angle (o) |
1/28/2019 | I11901 | 110 | 1.35 |