Difference between revisions of "YES-SPR220-Various-Temps"
Jump to navigation
Jump to search
Line 2: | Line 2: | ||
[[File:YES-SPR220vsTemp.jpg|578x578px]] |
[[File:YES-SPR220vsTemp.jpg|578x578px]] |
||
+ | |||
+ | <br /> |
||
+ | [[File:PPR220-7 Etch Rates vs Temperature.jpg|left|thumb|572.812x572.812px|Positive PR 220-7 etch rates vs set point temperature]] |
||
+ | |||
<br /> |