Difference between revisions of "YES-SPR220-Various-Temps"

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(add O2 only comment)
 
Line 1: Line 1:
 
Pressure drop indicates completion of etch. Once pressure flattens etching is complete.
 
Pressure drop indicates completion of etch. Once pressure flattens etching is complete.
   
[[File:YES-SPR220vsTemp.jpg|578x578px]]
+
[[File:YES-SPR220vsTemp.jpg|578x578px]]<br />
[[File:PPR 220-7 Etch Rates vs Temperature.jpg|left|thumb|572x572px|alt=|Oxygen only recipes, 3KW power, O2 2000sccm]]
 
<br />
 

Latest revision as of 09:53, 5 June 2023

Pressure drop indicates completion of etch. Once pressure flattens etching is complete.

YES-SPR220vsTemp.jpg