Filmetrics F40-UV Microscope-Mounted: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
m tool descr. update |
m punctiation of tool type |
||
| Line 2: | Line 2: | ||
|super = Ning Cao |
|super = Ning Cao |
||
|picture=Filmetrics F40-UV - system pic 01.jpg |
|picture=Filmetrics F40-UV - system pic 01.jpg |
||
|type = Inspection, |
|type = Inspection, Test and Characterization |
||
|location = Bay #4 |
|location = Bay #4 |
||
|description = Microscope-mounted optical reflectometry |
|description = Microscope-mounted optical reflectometry |
||
Revision as of 07:03, 24 May 2019
|
About
The Filmetrics F40-UV is a microscope-mounted thin-film measurement system, allowing you to non-destructively measure thin-film thicknesses in small (patterned) areas on your sample. It is an optical reflectometer, acquiring reflection spectra between 400-900nm optical wavelengths (Vis to Near-IR) with a regular halogen microscope light source. The Filmetrics software then performs curve-fitting to determine the thickness and/or refractive index of the measured films.
Capabilities
- Measure optically transparent thin-films down to ~30nm thickness.
- Microscope Objectives: 10x, 20x, 50x, 100x, 150x
- Acquire Optical Reflection Spectra from 400-900nm
- Spectrometer/Detector is capable of detecting down to UV ~190nm, but light source does not support this wavelength.
- Reflectivity curve-fitting for thin-film thickness analysis, supporting many common materials (Si3N4, SiO2 dielectrics, Si, GaAs, InP semiconductors, metals, photoresists etc.)