The Eight-Target DC/RF Sputtering System, built by AJA International uses planar magnetron sources. The sputter guns are in-situ tiltable modules that allow for maintaining uniformity control at various sample heights. Cross contamination between sources is minimized by using a "chimney" configuration with very narrow source to shutter gaps. Uniformity better than 2% is achieved for various sample heights. 4 DC and 1 RF power supplies allow for co-deposition of materials as well as the sputtering of a wide variety of materials. Other materials, such as ITO, Si, Al, Zr, etc. can be reactively RF sputtered in an O<sub>2</sub> or N<sub>2</sub> environment to produce metal-oxides or nitrides. The deposition chamber is loadlocked, with automatic wafer transfer, providing for fast substrate transfer and consistent, low base pressure. Venting and evacuation are automated with a 1000 l/s turbo pump achieving < 1 E-7 T ultimate pressure. A VAT gate valve is used for process pressure control independent of gas flow. Flow rates are controlled with standard mass flow controllers. Argon is used for the sputter gas, with N<sub>2</sub> and O<sub>2</sub> used for reactive sputtering.Substrates are clip mounted onto the carriers. Gun power supplies include: 300W DC, 13.56 Mhz 300W RF, and a 150W substrate RF supply for in-situ substrate biasing and pre-cleaning. Samples can be heated to 800°C. The system is recipe driven and computer controlled for reproducible results. Up to 6" round wafer sizes can be accomodated in the system.
The Eight-Target DC/RF Sputtering System, built by AJA International uses planar magnetron sources. The sputter guns are in-situ tiltable modules that allow for maintaining uniformity control at various sample heights. Cross contamination between sources is minimized by using a "chimney" configuration with very narrow source to shutter gaps. Uniformity better than 2% is achieved for various sample heights. 4 DC and 1 RF power supplies allow for co-deposition of materials as well as the sputtering of a wide variety of materials. Other materials, such as ITO, Si, Al, Zr, etc. can be reactively RF sputtered in an O<sub>2</sub> or N<sub>2</sub> environment to produce metal-oxides or nitrides. The deposition chamber is loadlocked, with automatic wafer transfer, providing for fast substrate transfer and consistent, low base pressure. Venting and evacuation are automated with a 1200 l/s turbo pump achieving < 5 E-8T ultimate pressure. A VAT gate valve is used for process pressure control independent of gas flow. Flow rates are controlled with standard mass flow controllers. Argon is used for the sputter gas, with N<sub>2</sub> and O<sub>2</sub> used for reactive sputtering.Substrates are clip mounted onto the carriers. Gun power supplies include: 300W DC, 13.56 Mhz 300W RF, and a 150W substrate RF supply for in-situ substrate biasing and pre-cleaning. Samples can be heated to 800°C. The system is recipe driven and computer controlled for reproducible results. Up to 6" round wafer sizes can be accomodated in the system.


===== Heading text =====
===== Heading text =====

Revision as of 16:24, 20 April 2020

Sputter 5 (AJA ATC 2200-V)
Tool Type Vacuum Deposition
Location Bay 3
Supervisor Tony Bosch
Supervisor Phone (805) 893-3486
Supervisor E-Mail bosch@ece.ucsb.edu
Description 8 Gun Sputtering System
Manufacturer AJA ATC 2200-V
Vacuum Deposition Recipes



About

The Eight-Target DC/RF Sputtering System, built by AJA International uses planar magnetron sources. The sputter guns are in-situ tiltable modules that allow for maintaining uniformity control at various sample heights. Cross contamination between sources is minimized by using a "chimney" configuration with very narrow source to shutter gaps. Uniformity better than 2% is achieved for various sample heights. 4 DC and 1 RF power supplies allow for co-deposition of materials as well as the sputtering of a wide variety of materials. Other materials, such as ITO, Si, Al, Zr, etc. can be reactively RF sputtered in an O2 or N2 environment to produce metal-oxides or nitrides. The deposition chamber is loadlocked, with automatic wafer transfer, providing for fast substrate transfer and consistent, low base pressure. Venting and evacuation are automated with a 1200 l/s turbo pump achieving < 5 E-8T ultimate pressure. A VAT gate valve is used for process pressure control independent of gas flow. Flow rates are controlled with standard mass flow controllers. Argon is used for the sputter gas, with N2 and O2 used for reactive sputtering.Substrates are clip mounted onto the carriers. Gun power supplies include: 300W DC, 13.56 Mhz 300W RF, and a 150W substrate RF supply for in-situ substrate biasing and pre-cleaning. Samples can be heated to 800°C. The system is recipe driven and computer controlled for reproducible results. Up to 6" round wafer sizes can be accomodated in the system.

Heading text