Surface Analysis (KLA/Tencor Surfscan): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(added exmaple of low particle count)
No edit summary
Line 1: Line 1:
{{tool|{{PAGENAME}}
{{tool2|{{PAGENAME}}
|picture=KLA.jpg
|picture=KLA.jpg
|type = Inspection, Test and Characterization
|type = Inspection, Test and Characterization
|super= Biljana Stamenic
|super= Biljana Stamenic
|super2= Don Freeborn
|location=Bay 5
|location=Bay 5
|description = Surface Analysis
|description = Surface Analysis

Revision as of 19:00, 30 August 2022

Surface Analysis (KLA/Tencor Surfscan)
KLA.jpg
Location Bay 5
Tool Type Inspection, Test and Characterization
Manufacturer Tencor
Description Surface Analysis
KLA/Tencor Surfscan

Primary Supervisor Biljana Stamenic
(805) 893-4002
biljana@ece.ucsb.edu

Secondary Supervisor

Don Freeborn


Recipes


About

This system uses a laser-based scattering method to count size and distribution of particles (or other scattering defects) on a flat wafer surface. It can scan wafers in size from 4 to 8 inches.

Documentation


Examples


A low-particle 4-inch wafer example:
Gain 4: Small Particles

(0.160µm – 1.60µm)

Gain 2: Large Particles

(1.60µm – 28.0µm)

Surfscan Low-Particle Example - G4.png Surfscan Low-Particle Example - G2.png
A high-particle 4-inch wafer example:
Gain 4: Small Particles

(0.160µm – 1.60µm)

Gain 2: Large Particles

(1.60µm – 28.0µm)

To Be Added To Be Added