High Temp Oven (Blue M): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
No edit summary
(Added operating procedures)
 
(One intermediate revision by one other user not shown)
Line 1: Line 1:
{{tool|{{PAGENAME}}
{{tool2|{{PAGENAME}}
|picture=BlueMOven.jpg
|picture=BlueMOven.jpg
|type = Lithography
|type = Lithography
|super= Brian Lingg
|super= Michael Barreraz
|super2= Aidan Hopkins
|location=Bay 5
|location=Bay 5
|description = High Temperature Oven
|description = High Temperature Oven
|manufacturer = Blue M Electric
|manufacturer = Blue M Electric
|toolid=56
|toolid=56
}}
}}The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.
The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.


Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.
Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.

<br />

== Operating Procedures ==


[https://wiki.nanotech.ucsb.edu/w/images/6/6c/BlueM_Instructions.pdf BlueM Oven Instructions]

Latest revision as of 17:33, 8 September 2022

High Temp Oven (Blue M)
BlueMOven.jpg
Location Bay 5
Tool Type Lithography
Manufacturer Blue M Electric
Description High Temperature Oven

Primary Supervisor Michael Barreraz
(805) 893-4147
mikebarreraz@ece.ucsb.edu

Secondary Supervisor

Aidan Hopkins


Recipes

SignupMonkey: Sign up for this tool


The Blue M oven has a Nitrogen purge (manual flow) and is able to be programmed for a series of custom temperature ramps and holds, with a maximum temperature of 350°C. It is not actively cooled.

Numerous spin-on dielectrics and polymers are often cured in this oven, such as BCB, SU-8 and Polyimide.


Operating Procedures

BlueM Oven Instructions