YES Recipe Screenshots: STD-O2: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
screenshots of "STD-O2-180C-3KW-30sec" and "STD-O2-100C-3KW-15min"
 
(No difference)

Latest revision as of 19:12, 30 November 2023

STD-O2-100C-3KW-15min
Header Steps
screenshot of STD-O2-100C-3KW-15min - header
STD-O2-100C-3KW-15min - header
screenshot of STD-O2-100C-3KW-15min - steps
STD-O2-100C-3KW-15min - steps
STD-O2-180C-3KW-30sec
Header Steps
screenshot of STD-O2-180C-3KW-30sec - header
STD-O2-180C-3KW-30sec - header
screenshot of STD-O2-180C-3KW-30sec - steps
STD-O2-180C-3KW-30sec - steps