DUV Flood Expose: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
(System model and manufacturer info)
(SOP Rev)
 
(3 intermediate revisions by 2 users not shown)
Line 1: Line 1:
<br />{{tool2|{{PAGENAME}}
<nowiki>&lt;nowiki&gt;Insert non-formatted text here</nowiki><nowiki>&lt;nowiki&gt;Insert non-formatted text here</nowiki>&lt;/nowiki&gt;&lt;/nowiki&gt;{{tool|{{PAGENAME}}
|picture=DUV.jpg
|picture=DUV.jpg
|type = Lithography
|type = Lithography
|super= Lee Sawyer
|super= Lee Sawyer
|super2= Bill Millerski
|phone=(805)893-2123
|phone=(805)893-2123
|location=Bay 6
|location=Bay 6
Line 11: Line 12:
}}
}}


= About =
==About==
This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter.
This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter.


Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc.
Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc.


=Detailed Specifications=
==Detailed Specifications==

*DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 watts and can operate in either constant intensity or constant power mode
*DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 watts and can operate in either constant intensity or constant power mode
*The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample
*The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample
Line 22: Line 24:
*Lamps are nominally rated for 400 hours
*Lamps are nominally rated for 400 hours
*A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation
*A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation
=Spectra Images=


==Spectra Images==
==DUV Exposure System Spectra==

===DUV Exposure System Spectra===
[[image:DUV-System-Spectra.png|thumb|none|600px|DUV Exposure System Spectra]]
[[image:DUV-System-Spectra.png|thumb|none|600px|DUV Exposure System Spectra]]

==Documentation==

*[https://wiki.nanofab.ucsb.edu/w/images/8/89/DUV_Flood_Expose_SOP_Rev_C.pdf DUV Flood Expose Standard Operating Procedure]

Latest revision as of 22:40, 4 January 2024


DUV Flood Expose
DUV.jpg
Location Bay 6
Tool Type Lithography
Manufacturer Bachur & Associates/AB Manufacturing
Description 1000W Deep UV Flood Exposure System (LS-150X-10C2) and Illumination Controller (2130-C2)

Primary Supervisor Lee Sawyer
(805) 893-2123
lee_sawyer@ucsb.edu

Secondary Supervisor

Bill Millerski


Recipes


About

This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter.

Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc.

Detailed Specifications

  • DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 watts and can operate in either constant intensity or constant power mode
  • The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample
  • Exposure can be performed on a 4" wafer
  • Lamps are nominally rated for 400 hours
  • A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation