==Detailed Specifications== |
==Detailed Specifications== |
||
*DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 |
*DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 Watts and can operate in either constant intensity or constant power mode |
||
*The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample |
*The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample |
||
*Exposure can be performed on a 4" wafer |
*Exposure can be performed on a 4" wafer |
||
Line 32: | Line 32: | ||
==Documentation== |
==Documentation== |
||
*[https:// |
*[https://wiki.nanofab.ucsb.edu/w/images/8/89/DUV_Flood_Expose_SOP_Rev_C.pdf DUV Flood Expose Standard Operating Procedure] |
Latest revision as of 01:55, 13 May 2025
|
About
This unit consists of a collimated deep ultraviolet (DUV) light source (mercury gas discharge short arc lamp) and power supply. The substrate is placed on a rotating chuck (not presently working) and is exposed by opening a timer-controlled shutter.
Materials that are exposed are primarily spun-on thin films such as PMMA, PMGI, etc.
Detailed Specifications
- DUV wavelengths are 200-260 nm; the lamp power is limited to 1000 Watts and can operate in either constant intensity or constant power mode
- The full spectrum of Hg emission wavelengths from 200-450 nm is present on the sample
- Exposure can be performed on a 4" wafer
- Lamps are nominally rated for 400 hours
- A reset timer was added in Feb. 1995 to limit "on" time (ie. provide for auto shut-off) for bulb life conservation