Gold Plating Bench (Semcon): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
Created page with "{{tool|{{PAGENAME}} |picture=GoldPlating.jpg |type = Wet Processing |super= Tony Bosch |phone=(805)839-3918x217 |location=Bay 5 |email=bosch@ece.ucsb.edu |description = Technic A…" |
m John d moved page Gold Plating Bench to Gold Plating Bench (Semcon): adding mfg name, to differentiate it being just a wet bench. |
||
| (3 intermediate revisions by 2 users not shown) | |||
| Line 9: | Line 9: | ||
|manufacturer = [http://www.technic.com/ Technic, Inc.] |
|manufacturer = [http://www.technic.com/ Technic, Inc.] |
||
|materials = |
|materials = |
||
|model=SEMCON 1000 |
|||
|toolid=48 |
|||
}} |
}} |
||
= |
==About== |
||
The Technic SEMCON 1000 plating system is a single cell plating bath using chemistry suitable for gold plating through vias in resist or on other flat and structured samples with reasonable rates, resistivity, and stress. Films from tenths of a micron to 10s of microns can be plated on a variety of substrate sizes. |
The Technic SEMCON 1000 plating system is a single cell plating bath using chemistry suitable for gold plating through vias in resist or on other flat and structured samples with reasonable rates, resistivity, and stress. Films from tenths of a micron to 10s of microns can be plated on a variety of substrate sizes. |
||
== Recipes == |
|||
'''Recipes > Wet Processing > [[Wet Etching Recipes#Gold Plating Bench .28Technic SEMCON 1000.29|Gold Plating (SEMCON 100)]]''' has starter recipes for this tool. |
|||
Latest revision as of 20:48, 15 August 2025
|
About
The Technic SEMCON 1000 plating system is a single cell plating bath using chemistry suitable for gold plating through vias in resist or on other flat and structured samples with reasonable rates, resistivity, and stress. Films from tenths of a micron to 10s of microns can be plated on a variety of substrate sizes.
Recipes
Recipes > Wet Processing > Gold Plating (SEMCON 100) has starter recipes for this tool.