Template:Announcements: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
THERMco furnace up, deleted DSEiii
deleted xmas shutdown
 
(874 intermediate revisions by 8 users not shown)
Line 1: Line 1:
<startfeed />
<startfeed />

<!--feedBurner name="UCSBNanofab-Announcements" /-->
=====Announcements moved=====
<!-- Description of the RSS feed -->
Please check the <u>[https://signupmonkey.ece.ucsb.edu announcements in SignupMonkey]</u> for equipment notifications.
''UCSB NanoFab Announcements''
// [[User:John_d|Demis D. John]] 02:03, 27 November 2025 (UTC)

<!--
<!--
SEE THE BOTTOM OF THIS PAGE FOR INSTRUCTIONS ON ADDING NEWS ITEMS.
SEE THE BOTTOM OF THIS PAGE FOR DETAILED INSTRUCTIONS ON ADDING NEWS ITEMS.
In order for your post to show up correctly, you need to:
>> Use FIVE equal-signs for the Title's heading level. eg.: ===== my post =====
>> Use two slashes // and FOUR tilde's to insert your signature at the end of your post: //~~~~
-->
-->
<!---------------------------------------------->
<!---------DO NOT EDIT BELOW THIS LINE----------->
<!------------- Announcements ---------------->

===== SEM#2: Down =====
The loading arm has been damaged beyond simple repair.
JEOL is overnighting us a new load arm.
We should receive the arm sometime late morning tomorrow so if the install goes
well (and there is no other damage to the tool) the SEM should be
available to use Friday afternoon.
// [[User:John d|John d]] 11:33, 26 July 2018 (PDT)

===== Wafer Bonding Furnace is UP =====
Wafer Bonding Tube Furnace (Thermco), is now UP.
// [[User:John d|John d]] 11:35, 26 July 2018 (PDT)

===== Ebeam#2: heater inoperable =====
The heater is damaged beyond our ability to repair it. We have contacted
the vendor and asked for an "expedited" repair if possible.
// [[User:John d|John d]] 13:51, 25 July 2018 (PDT)

===== Sputter #3 UP =====
We have installed and tested the new solenoid block. Still, make sure to verify the XFER valve is CLOSED before you vent the Loadlock.
// [[User:John d|John d]] 11:49, 24 July 2018 (PDT)

===== PECVD#1: Software Upgrade =====
We are going to upgrade the computer and software on PECVD#1 in 2–3 weeks. The tool will be down for three to five days. Once the upgrade is complete, everyone will need to be retrained on the new software. You should start planning accordingly, if you use this tool. We will send out an email when we know the exact dates.
// [[User:John d|John d]] 15:05, 20 June 2018 (PDT)

===== RIE#5: SiCl4 Issue =====
We have a flow rate problem on the SiCl4 gas line. You can only flow the SiCl4 for 5 minutes and then you have to wait 5 minutes before you flow it again. So in order to to do a 10 minute Etch you will have to do it in three steps flow 5 mi, wait 5mi, then flow 5min.
// [[User:John d|John d]] 17:22, 15 June 2018 (PDT)

<!---------- end of announcements ------------>
<!---------------------------------------------->
<endfeed />
<endfeed />
<noinclude>[[Category:Templates]]</noinclude>
<noinclude>[[Category:Templates]]</noinclude>
<!--------------------------------------------
<!--------------------------------------------
====== HOW TO ADD ITEMS ======

* You can copy/paste the example below for a new news item.



====== HOW TO ADD NEWS ITEMS ======

* Use level 5 heading for each item (5 equal signs surrounding the title) - they will show up as separate RSS items this way. (This looks best on the Wiki homepage)
* Use level 5 heading for each item (5 equal signs surrounding the title) - they will show up as separate RSS items this way. (This looks best on the Wiki homepage)
* You must add a user signature at the end of each post via four tildes: ~~~~. Required for the RSS plugin to determine the timestamp, or else post goes to the end of the RSS feed.
* You must add a user signature at the end of each post via four tildes: [[User:Silva|Silva]] 13:26, 4 February 2023 (PST). Required for the RSS plugin to determine the timestamp, or else post goes to the end of the RSS feed.
* Use double-slash: // at start of new lines - makes display on the Samsung Display look a lot better, since it strips newlines.
* Use double-slash: // at start of new lines - makes display on the Samsung Display look a lot better, since it strips newlines.
* Optional: After saving the page, delete the name after the two dashes "--" and delete the "[[(talk)...]]" link.
* Optional: After saving the page, delete the name after the two dashes "--" and delete the "[[(talk)...]]" link.
* Please use "There are no announcements at this time." if the announcements are empty.
* Please use "There are no announcements at this time." if the announcements are empty.

* URL to the RSS feed via FeedBurner (for Samsung display): http://wiki.nanotech.ucsb.edu/w/index.php?title=Template:Announcements&action=feed&feed=rss
* URL to the RSS feed directly from Wiki: https://wiki.nanotech.ucsb.edu/w/index.php?title=Template:Announcements&action=feed&feed=rss




Line 60: Line 31:
===== NanoFab making LN2 icecream =====
===== NanoFab making LN2 icecream =====
Tomorrow the NanoFab will be serving liquid nitrogen ice cream.
Tomorrow the NanoFab will be serving liquid nitrogen ice cream.
// [[User:Silva|Silva]] 13:26, 4 February 2023 (PST)
// ~~~~


(end of example)
************* (end of example) **************
The ~~~~ will be replaced with your username & timestamp after you submit the post.
The [[User:Silva|Silva]] 13:26, 4 February 2023 (PST) will be replaced with your username & timestamp after you submit the post.
---------------------------------------------->
---------------------------------------------->

Latest revision as of 19:31, 5 February 2026

Announcements moved

Please check the announcements in SignupMonkey for equipment notifications. // Demis D. John 02:03, 27 November 2025 (UTC)