Created page with "{{tool|{{PAGENAME}} |picture=Oven4.jpg |type = Lithography |super= Tony Bosch |location=Bay 6 |description = ? |manufacturer = Fisher Scientific }}" |
fixed instructions link |
||
| (8 intermediate revisions by 4 users not shown) | |||
| Line 1: | Line 1: | ||
{{ |
{{tool2|{{PAGENAME}} |
||
|picture=Oven4.jpg |
|picture=Oven4.jpg |
||
|type = Lithography |
|type = Lithography |
||
|super= |
|super= Michael Barreraz |
||
|super2= Aidan Hopkins |
|||
|location=Bay 6 |
|location=Bay 6 |
||
|description = |
|description = Programmable Oven |
||
|manufacturer = |
|manufacturer = Thermo Scientific |
||
|model = HeraTherm |
|||
|toolid=68 |
|||
}} |
}} |
||
==About== |
|||
This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven. |
|||
==Specifications== |
|||
*Maximum Temperature = 330 C (no active cooling) |
|||
*Gases: N2, manually set with needle valve (not programmable) |
|||
*Multi-step programmable temperature ramps |
|||
*Programmable atmospheric purge (for cooling) |
|||
==Documentation== |
|||
* [https://wiki.nanotech.ucsb.edu/w/images/8/8e/Heratherm_instructions.pdf Instructions (from HeraTherm)] |
|||
<br /> |
|||
Latest revision as of 20:04, 25 February 2026
| ||||||||||||||||||||||||||||||||
About
This oven is often used for long thermal cures and wafer bonding. It has programmable temperature ramps and hold times, but the ramp rate is only "low/med./high" (not an exact ramp rate). A manual needle valve for nitrogen purge has been installed on the back of the oven.
Specifications
- Maximum Temperature = 330 C (no active cooling)
- Gases: N2, manually set with needle valve (not programmable)
- Multi-step programmable temperature ramps
- Programmable atmospheric purge (for cooling)
Documentation