PECVD 2 (Advanced Vacuum): Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Process Control Data: added process control images etc.
Barreraz (talk | contribs)
 
(One intermediate revision by one other user not shown)
Line 37: Line 37:
*
*
*
*
*[https://wiki.nanotech.ucsb.edu/w/images/2/2c/SOP_for_Advanced_Vacuum_PECVD.pdf Operating Instructions]
*[https://wiki.nanofab.ucsb.edu/w/images/9/9a/PECVD2_SOP_Final_V45.47_3-6-26-compressed.pdf Operating Instructions]
*[https://wiki.nanofab.ucsb.edu/w/images/6/68/PECVD2_STD_LS_Si3N4v4recipe_depositiontime.pdf Modifying Deposition Time in "STD LS-Si3N4v4" Recipe]
*[https://wiki.nanofab.ucsb.edu/w/images/6/68/PECVD2_STD_LS_Si3N4v4recipe_depositiontime.pdf Modifying Deposition Time in "STD LS-Si3N4v4" Recipe]
*[https://wiki.nanofab.ucsb.edu/w/images/1/1b/PECVD2_Recipe_Temperature_Change.pdf Modifying Deposition Temperature]
*[https://wiki.nanofab.ucsb.edu/w/images/1/1b/PECVD2_Recipe_Temperature_Change.pdf Modifying Deposition Temperature]
Line 50: Line 50:
*Standard Recipes: [[PECVD Recipes#PECVD 2 .28Advanced Vacuum.29|'''Recipes > Deposition > <u>PECVD #2</u>''']]
*Standard Recipes: [[PECVD Recipes#PECVD 2 .28Advanced Vacuum.29|'''Recipes > Deposition > <u>PECVD #2</u>''']]


*A list of ''all available'' deposited films can be found on the Vacuum Deposition Recipes page:
*A list of ''all available'' deposited films can be found here: [[Vacuum Deposition Recipes|Recipes > Vacuum Deposition Recipes]]
**[[Vacuum Deposition Recipes|Recipes > Vacuum Deposition Recipes]]


===Process Control Data===
===Process Control Data===

Latest revision as of 18:55, 6 March 2026

PECVD 2 (Advanced Vacuum)
Location Bay 2
Tool Type Vacuum Deposition
Manufacturer Plasma-Therm
Description Vision 310 Advanced Vacuum PECVD

Primary Supervisor Michael Barreraz
(805) 893-4147
mikebarreraz@ece.ucsb.edu

Secondary Supervisor

Don Freeborn


Recipes Vacuum Deposition Recipes

SignupMonkey: Sign up for this tool


About

  • Films/Gases: This open-load system is dedicated to PECVD of SiO2, SiNx, SiOxNy, and a-Si using Silane (2%SiH4, 98% He), N2O, NH3, and N2 gases.
  • Size: The sample electrode has a 270mm diameter useable area, allowing for multiple 4” wafer depositions in a single run.
  • Temperature: Standard operating temperature is 300C, but can be user changed for temps ranging anywhere from 250 to 350C.
  • Low-Stress Si3N4: The system is equipped with a dual generator, dual frequency option for growth of Low-stress Nitride films.
    • These films alternate between thin (<10nm) compressive and tensile layers.
    • The Low-Stress Si3N4 film recipe are tested approx. monthly, and kept within ±100MPa. Data can be found at Recipes (below) > Low-Stress Nitride.

See Also

Documentation

Recipes & Data

SPC chart example
Example Process Control Charts (SPC) for thin-film DepCals.
screenshot of surfscan particle count
Example particle counts taken on each film.
Screenshot of Filmetrics F50 wafermap of typical DepCals film
Example of DepCals Thickness/Refractive Index uniformity measurement (4% shown here).

Process Control Data