Vacuum Sealer: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
Silva (talk | contribs)
No edit summary
addedc both sealers, info on suppllies and logn term storage with dessicant
 
(One intermediate revision by one other user not shown)
Line 1: Line 1:
{{tool|{{PAGENAME}}
{{tool2|{{PAGENAME}}
|picture=Vacuum.jpg
|picture=Vacuum.jpg
|type = Packaging
|type = Packaging
|super= Don Freeborn
|super= Michael Barreraz
|super2= Aidan Hopkins
|location=Bay 4
|location=Bay 4
|description = ?
|description = ?
|manufacturer = ?
|manufacturer = ?
}}
}}

= About =
== About ==

To prevent samples from oxidizing, we have two vacuum sealers, silica dessicant packets and aluminum foil coated bags.

== Mini-pack Torre Vacuum Sealer ==

Larger chamber, can accommodate 100mm cassettes of 150mm individual wafer trays.

== Food Vacuum Sealer ==

[[File:Vacuum Sealer photo IMG 9946.png|link=https://wiki.nanofab.ucsb.edu/wiki/File:Vacuum%20Sealer%20photo%20IMG%209946.png|alt=Bonsen Kitchen vacuum sealer photo|none|thumb|280x280px]]Perfect for small wafer trays, very easy to use and fast.

== Bags + Dessicant packets ==

We provide silica dessicant packets, which you should place inside your bag to absorb water.

Plastic bags are provided at various sizes. For short-term (eg. few-month) storage these will work. However water-vapor does diffuse through plastic over time (eg. months).

For long-term storage, it is recommended to use the Aluminum-coated bags, which block diffusion of water & oxygen. Combined with dessicant packets, this should provide a good long-term storage solution for wafers sensitive to atmospheric water (eg. with Aluminum-containing epitaxial layers).

Latest revision as of 17:22, 30 April 2026

Vacuum Sealer
Location Bay 4
Tool Type Packaging
Manufacturer ?
Description ?

Primary Supervisor Michael Barreraz
(805) 893-4147
mikebarreraz@ece.ucsb.edu

Secondary Supervisor

Aidan Hopkins


Recipes


About

To prevent samples from oxidizing, we have two vacuum sealers, silica dessicant packets and aluminum foil coated bags.

Mini-pack Torre Vacuum Sealer

Larger chamber, can accommodate 100mm cassettes of 150mm individual wafer trays.

Food Vacuum Sealer

Bonsen Kitchen vacuum sealer photo

Perfect for small wafer trays, very easy to use and fast.

Bags + Dessicant packets

We provide silica dessicant packets, which you should place inside your bag to absorb water.

Plastic bags are provided at various sizes. For short-term (eg. few-month) storage these will work. However water-vapor does diffuse through plastic over time (eg. months).

For long-term storage, it is recommended to use the Aluminum-coated bags, which block diffusion of water & oxygen. Combined with dessicant packets, this should provide a good long-term storage solution for wafers sensitive to atmospheric water (eg. with Aluminum-containing epitaxial layers).