MLA150 - CAD Files and Templates: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
→Resolution and Calibration Patterns: details on CAD files available on MLA150 computer
 
(One intermediate revision by the same user not shown)
Line 1: Line 1:
==Alignment Marks==
==Alignment Marks==
⚫
Alignment Crosses can be exposed by the MLA150 itself (good for full wafers with open areas on the edges) using the ''Expose Bitmaps'' field in the Job Setup, or can be included in your CAD file (good for smaller pieces without much unused edge area).

Any cross shape with a 10-50µm wide line will work for automatic alignment. By default, system expects this cross shape to cover/extend beyond the entire field of view of the chosen microscope, which are the following sizes:
Any cross shape with a 10-50µm wide line will work for automatic alignment. By default, system expects this cross shape to cover/extend beyond the entire field of view of the chosen microscope, which are the following sizes:
{| class="wikitable"
{| class="wikitable"
Line 15: Line 17:


The coordinates to the center of each mark should be known, with respect to the origin (0,0) of the CAD file to be exposed.
The coordinates to the center of each mark should be known, with respect to the origin (0,0) of the CAD file to be exposed.

⚫
Crosses can be exposed by the MLA150 itself (good for full wafers with open areas on the edges), or can be included in your CAD file (good for cleaved pieces without much unused edge area).


==Resolution and Calibration Patterns==
==Resolution and Calibration Patterns==
Line 28: Line 28:
**Image Size for the Unit-Cell: 500 x 650µm for stitching the alignment crosses of adjacent die.
**Image Size for the Unit-Cell: 500 x 650µm for stitching the alignment crosses of adjacent die.
*''UCSB_MLA150_Calibration_pattern_v5_AcrossWafer.gds'' - covers a 100mm wafer, used for alignment vernier testing.
*''UCSB_MLA150_Calibration_pattern_v5_AcrossWafer.gds'' - covers a 100mm wafer, used for alignment vernier testing.

==Other CAD File Templates==
See the [[Calculators + Utilities#CAD%20Files%20.26%20Templates|Calculators + Utilities > CAD Files & Templates]] page for other useful CAD files, such as overlay verniers, vented fonts etc.

Latest revision as of 04:25, 5 April 2024

Alignment Marks

Alignment Crosses can be exposed by the MLA150 itself (good for full wafers with open areas on the edges) using the Expose Bitmaps field in the Job Setup, or can be included in your CAD file (good for smaller pieces without much unused edge area).

Any cross shape with a 10-50µm wide line will work for automatic alignment. By default, system expects this cross shape to cover/extend beyond the entire field of view of the chosen microscope, which are the following sizes:

Alignment mark sizes should be larger than the following
Camera Field of View
Low Mag. 640 x 480 µm
High Mag. 190 x 140 µm

For the best alignment, the High-Mag camera is preferred, so a Cross of ~250µm x 200µm (50µm larger than the high-mag. FOV), with line width of 20µm would be acceptable.

The coordinates to the center of each mark should be known, with respect to the origin (0,0) of the CAD file to be exposed.

Resolution and Calibration Patterns

Resolution test patterns and Alignment Verniers can be found on the local MLA150 computer in the .../Users-Nanofiles/a-Public Templates folder.

Has line-space resolutions from 65nm → 1.0µm. Isolated versus dense lines are shown via lines protruding further beyond the dense patterns. The text indicates the "period" - twice the line/space width.

You will find two such files on the tool:

  • UCSB_MLA150_Calibration_pattern_v5_UnitCell.gds - a single unit cell of the pattern, used for focus-exposure matrix (series)
    • Image Size for the Unit-Cell: 500 x 650µm for stitching the alignment crosses of adjacent die.
  • UCSB_MLA150_Calibration_pattern_v5_AcrossWafer.gds - covers a 100mm wafer, used for alignment vernier testing.

Other CAD File Templates

See the Calculators + Utilities > CAD Files & Templates page for other useful CAD files, such as overlay verniers, vented fonts etc.