Template:Announcements: Difference between revisions

From UCSB Nanofab Wiki
Jump to navigation Jump to search
Content deleted Content added
→Tools that are currently down: title --> tool updates, use dbl-slash // delimit
→Tool Updates: cary 500 update
Line 25: Line 25:
// GCA 6300 Stepper #1:
// GCA 6300 Stepper #1:
Lamp power supply failure. Replacement is being shipped.
Lamp power supply failure. Replacement is being shipped.

// Cary 500:
UV-Vis Detector Failure. Locating replacement.


// [[User:John d|Posted:]] 15:06, 7 December 2017 (PST)
// [[User:John d|Posted:]] 15:06, 7 December 2017 (PST)

Revision as of 04:33, 8 December 2017

Announcements

The NanoFab has reopened, as power appears to have stabilized.

The Thomas Fire & Rye Fire in Ventura County caused repeated power outages on the evening of Monday 12/4. CalFire is posting updates on their webpage and FaceBook page.

Posted: 15:07, 7 December 2017 (PST)

Tool Updates

// Panasonic ICP #1: Pump failed. Don is installing a replacement.

// GCA 6300 Stepper #1: Lamp power supply failure. Replacement is being shipped.

// Cary 500: UV-Vis Detector Failure. Locating replacement.

// Posted: 15:06, 7 December 2017 (PST)