Template:Announcements: Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
→ICP#1: Down: up |
→JEOL SEM #2: Down: up temp. |
||
| Line 21: | Line 21: | ||
// [[User:John d|Posted:]] 01:32, 15 February 2018 (PST) |
// [[User:John d|Posted:]] 01:32, 15 February 2018 (PST) |
||
===== JEOL SEM #2: |
===== JEOL SEM #2: Up ===== |
||
System up for use. JEOL service ot return on Tues for permanent fix. |
|||
Load Lock problem. |
|||
// [[User:John d|Posted:]] |
// [[User:John d|Posted:]] 22:30, 16 February 2018 (PST) |
||
===== Gasonics: Up ===== |
===== Gasonics: Up ===== |
||
Revision as of 06:30, 17 February 2018
UCSB NanoFab Announcements
Announcements
There are no general announcements at this time. // Posted: 09:58, 4 January 2018 (PST)
ICP#1: Up
He cooling fixed. // Posted: 01:32, 15 February 2018 (PST)
JEOL SEM #2: Up
System up for use. JEOL service ot return on Tues for permanent fix. // Posted: 22:30, 16 February 2018 (PST)
Gasonics: Up
The process chamber mechanical pump is struggling to make base pressure but the system is able to successfully run. We are waiting for the replacement pump to repaired and returned. // Posted: 10:14, 12 February 2018 (PST)
Cary 500 Down
UV-Vis Detector Failure. Tool is able to used from 600nm and up. Looking into replacement options. // Posted: 13:47, 12 February 2018 (PST)