Test Data of etching SiO2 with CHF3/CF4/O2 (using this recipe only for Fluorine etch of the underneath layer): Difference between revisions
Jump to navigation
Jump to search
Content deleted Content added
add data |
add a pic |
||
| Line 29: | Line 29: | ||
|0.80 |
|0.80 |
||
|79.4 |
|79.4 |
||
|[https://www.nanotech.ucsb.edu/wiki/images/d/dc/SiO2_Etch_using_ICP2_with_O2-3-06-2019.pdf] |
|||
| |
|||
|} |
|} |
||